Finish your own guitar – and then relic it yourself
Those of you who have been following the Swedish magazine Musikermagasinet’s article series on assembling your own electric guitar from various parts have likely—just like me—wondered whether you couldn’t handle more of the aging process yourself. Throughout the series, we’ve tried our hand at “relicing” both plastic and metal components. Is it possible to do something similar with the guitar body? That’s what we’re going to find out today.
Christmas is just around the corner. Well, actually, maybe it isn’t… As I write this, it is only early November. But for those of you reading this article at home, the ordeal of the Christmas celebrations might already be over. Regardless of which issue this guide appears in, we are likely well past the holiday season. But this article isn’t about applying lacquer to Christmas presents. Instead, the idea is to try your hand at lacquering a guitar body yourself—and then “relicing” it to give it that perfectly worn-in look. “That’s a crazy idea!” I can already hear someone exclaim. And perhaps it is—but it’s a fun, and quite educational, kind of crazy. It might seem a bit mad to go to the trouble of prepping a guitar and applying a professional-grade lacquer finish, only to then undo all that hard work spent making the surface look as glossy and pristine as possible.
Well, I’ve made up my mind once and for all. Having assembled a number of Strat- and Telecaster-style guitars using wooden parts that had already been “relic’d” to just the right degree, I now feel a strong urge to try and achieve something similar on my own. After all, you end up paying quite a premium just to have someone else scrape up and ruin the finish on a guitar body—something you should actually be able to handle yourself, provided you have a bit of practice, a great deal of caution, plenty of self-confidence, and a wealth of useful information from both paint manufacturers and others who have attempted the same thing—and who have already made all the mistakes. The idea, of course, is to avoid having to pay for that part of the process if at all possible.
WE NEED A BODY
However, one piece we cannot avoid—or rather, one that we will need to sand—is the block of wood that will become the guitar body. In this instance, we essentially have to start from scratch. We won’t be sawing a body out of an old ash or alder tree; instead, we’ll need to track down a pre-cut Telecaster-style body from a retailer. If your local guitar shop doesn’t stock such items, you can certainly find one online or in the nearest major city. These days, you can actually find Telecaster bodies (or Stratocaster-style ones, if you prefer) at reasonable prices from various sources—both here in Sweden and abroad—provided you explore all the options available to you.

If you buy, for example, a top-quality pre-painted and reliculated telebody, it can cost around SEK 4-5,000. If you choose a completely unpainted body, and undertake to do the painting job yourself, you can easily get away with half the money, or even less. An alternative is to look out for used, or even brand new bodies, where the owner has already tired before starting the project. I have seen such wooden pieces both at *Blocket and in some more well-stocked music stores.
I was lucky enough to find a really nice, completely unfinished, one-piece ash body at my usual supplier for this sort of gear—No 1 Guitarshop, here in Gothenburg. It’s always an advantage to be able to get a feel for the piece of wood before committing to a purchase. And speaking of “committing,” it’s a good idea to hold the wooden body carefully and tap on it in various spots. This gives you a pretty clear picture of the quality of the wood you’ve got your hands on. If it “sings” when you tap it, it’s likely to keep singing once it’s been fitted with all the necessary components—the neck, tuners, bridge, and strings. If, on the other hand, it’s completely dead and dull, there’s a real risk that “dead and dull” will end up being the defining characteristic of the finished guitar. And that’s not exactly what you’re aiming for, is it?
Needless to say, I have absolutely no theoretical basis for these theories. It’s just something I’ve concluded after assembling half a dozen electric guitars.
PREPARATORY WORK
Once you have brought your new guitar body home, there is still quite a bit of work to be done before you can reach for the spray gun—or the spray can, if that is what you intend to use. The body needs to be sanded, and any cavities or other imperfections in the wood may benefit from the application of some grain filler. We are assuming here that you have a bare-wood body—that is, one that has not already been finished, which would require you to remove the old finish before starting. There are several types of grain filler available: water-based options (such as ColorTone Waterbase Grainfiller, sold by both gitarrdelar.se and stewmac.com), solvent-based products like Rustin’s Grain Filler (which is thinned with mineral spirits), or even pumice, which many guitar builders—including the phenomenal Åke Björnstad—frequently use.

I myself had fallen a little in love with the pictures of an old blonde ’52 in yellowed and nicely cracked butter-scotch cellulose varnish, where you could very clearly see all the grain and other things in the wood right through the varnish.
So I had decided early on not to refill these. I didn’t want a completely plain – and maybe a little impersonal – guitar body like that. My ideal was much closer to a worn John Mayer or Stevie Ray Vaughn Strat body – though perhaps still made with a little more restraint than these two fighters seem to have struggled to achive.
Looking back in, maybe it wouldn’t have totally wrong if I filled in a little of this veining on my Tele body as well. Decide for yourself how you want to do it. Maybe I was just a little too lazy, who knows? Next body I promise to fill the pores, shall we say so?
Anyway… The coarser the wood used for the guitar body, the more effort you need to put into the preparatory work—specifically pore filling and the subsequent sanding. Regardless of the type of pore filler you choose, the application method is generally the same: spread it along the grain first, then finish by working across it. Don’t apply too much, unless you want to sand yourself to death. And if you (like me) want the wood grain to show through a thin layer of finish, you can opt for a contrasting color for the pore filler—for instance, using a mahogany-colored filler on a lighter wood like ash.
When it comes to sanding, start with a relatively coarse-grit sandpaper and gradually work your way toward finer grits. I’ve seen a wide range of recommendations regarding grit size, but I believe it’s well worth putting in some extra effort here; start with something like 240 or 300 grit, then progress through the grades until you reach 600 or 1200 grit—or somewhere in that range. Use a solid sanding block, and be careful around the edges of the guitar.
Your best tool for determining when you’ve sanded enough is your own fingers. They can detect even the slightest unevenness; if it feels completely smooth to the touch, you can be confident that the result is excellent.
SPRAYING JOBS
You can buy cellulose lacquer—available in both spray cans and for use with a paint sprayer—from various sources, including both Swedish and international websites. The Swedish site Gitarrdelar.se offers a good selection of classic “Fender colors,” priced between 225 and 445 kronor, depending on the specific color. However, I received a tip (thanks, Fredrik at No 1 Guitars!) that Biltema carries a hobby paint based on cellulose lacquer, which costs only 59.90 kronor for a 400 ml spray can. They offer a fairly wide range of colors, though they aren’t labeled using the names of the old DuPont/Fender shades. I chose a light blue that was a shade darker than the “Daphne Blue” used by Fender and Cadillac, but it still looked quite good.

I estimated that I would need about two such cans, and I also decided to start with a white, semi-matte primer. If you like, you can then buy a clear coat to spray on as a final layer, which provides an even better sheen and more depth to the color. Either way, the cost to paint an entire guitar body comes to just a few hundred kronor.

When it comes to the lacquering process, I strongly recommend purchasing a good respirator (mask) and a pair of safety goggles. The mask, in particular, is absolutely essential! The lacquer has a very strong odor when sprayed, and it certainly contains solvents that are not exactly healthy! It is also a good idea to use disposable vinyl gloves.
In the past, Fender used nails to support the guitar body while the back was being sprayed. On vintage guitars, you can sometimes see the marks left by these nails underneath the pickguard. I opted for a simpler approach: I simply screwed a piece of wood into the neck pocket, using the same holes intended for the neck screws. This provided a convenient handle, allowing me to rotate the guitar while spraying it (see image).

When using spray cans from Biltema, there are a few things to keep in mind. Shake them very thoroughly, and avoid painting when it is too cold—though it is best to work outdoors, given the strong odor. If the can or the paint gets too cold, it tends to “spit,” which can result in unsightly spots in the finish. It may also end up looking a bit “hazy.” For instance, warm the spray can thoroughly in a bath of warm water before you begin the job. Apply a thin coat, wait a few seconds, and repeat the process a couple of times. Do not apply the paint too thickly; otherwise, it will easily run, which can be quite a hassle to fix later. While such issues can be sanded away, it is best to wait until all the coats of paint have been applied.
Let the paint dry for a day before spraying the next layer. You decide for yourself how many layers you want to lay. In my case, it was four (thin) layers of base color and (at least) six layers of the blue color. It sounds like a lot of layers, but remember that each layer is very thin. And you choose how you want to do with this.
Also, don’t forget to turn the can upside down after each finished spray, and thus clean the nozzle on the can by spraying until no more paint comes out.
TIME FOR POLISHING
The painting is now complete, and it is time to start polishing. However, it is best to let the finish harden for a couple of weeks before you begin sanding. This task requires a fair amount of “elbow grease”—as the expression goes in English-speaking countries. In other words, you’ll need to put in some hard work.

And speaking of grease, I also think you can continue to use the nice vinyl gloves. It costs almost nothing, and it’s always a good idea to keep grease and sweat from your hands away from the piece of wood, regardless of whether it’s plain wood or has a few layers of varnish. Most importantly, though, make sure you have a suitable surface on your workbench. A soft, moderately thick piece of fabric can work wonders in preventing debris on the workbench from leaving marks in the finish. While we do plan to “relic” the body later on, the final result is guaranteed to look better if the finish itself is flawless. And who knows—you might end up so pleased with the finish that you decide to postpone the relicing process, or skip it altogether. We shall see…
When it comes to polishing your new finish, wet-sanding paper is the way to go. It’s a good idea to keep a small bowl of water nearby—add a few drops of dish soap to it, and the sandpaper will work much more effectively.

It must not dry out completely, but you shouldn’t drench the guitar either. To be safe, you should seal all screw holes with wax or paper so that water doesn’t run into them; otherwise, you might end up with cracks when the guitar dries out later. Start with 400- or 600-grit sandpaper and work your way up. At first, the finish will look duller, but it will become glossier again as you move to finer grits. This is a stage where you can really pour your heart and soul into the work. If your usual sandpaper supplier doesn’t carry the finest grades, automotive supply stores often stock 1500- and 2000-grit paper, or finer still, should you wish to use them.

Once you feel you’re done sanding, it’s time for polishing—think of it like waxing your car. I actually picked up a small polisher with a sheepskin bonnet while I was shopping at Biltema. It only cost 249 kronor, and the results were extremely satisfying. Of course, you could also use a soft cloth and some elbow grease, but it’s much faster with a machine. Either way, you’ll end up with a nice, glossy finish.
THE RELIQUARY PROCESS
Now, let the lacquer harden thoroughly for a few weeks before moving on to the next step. Once the lacquering is finished and looks absolutely stunning, it can feel a bit daunting to start hacking and scraping at it to make it look worn. After all, once you’ve made that first scratch, there’s no turning back—it’s definitely too late to change your mind—so think this through very carefully before you begin.
But once you’ve made up your mind—and in my case, that’s what this whole article was supposed to be about—all you have to do is steel yourself, grab a screwdriver (or a set of old keys), and dive in. It’s a good idea to look at photos online; there are plenty of authentic images of vintage guitars—both Strats and Telecasters—that show you how, and above all where, the wear tends to appear. And remember: it’s always better to start by doing too little. You can always add more wear later, but it’s significantly harder (if not impossible) to undo what you’ve done—unless, of course, you happen to be incredibly skilled at retouching with nitrocellulose lacquer.


The first thing I did was drop a set of keys onto the guitar body several times, from various distances. Each time the keys landed, they created several small nicks, some scratches, and other similar marks. The beauty of these marks is that later on—when we go to crack the finish—the lacquer tends to crack specifically around these little nicks. This results in a network of hairline cracks that look extremely authentic.
After turning the guitar body over and letting the keys do their work on all sides, it’s time for some more substantial tools. I use a fairly heavy-duty, standard flat-head screwdriver. The blade is about 1 cm wide, but you can choose whatever you prefer.
Of course, you could take a more cautious approach, using sandpaper to gradually wear away the finish. But that often ends up looking more like “factory-made” wear than if you really go at it with a more substantial tool. Cellulose lacquer is quite brittle and delicate; the kind of nicks and scratches you see are typical—unless, that is, you’ve handled your guitar exclusively while wearing cotton gloves for the last 40 years. It’s easy for a screwdriver to slip while you’re adjusting the bridge intonation, and—presto—you’ve got a nice long scratch in the finish. That’s the sort of mistake we’re aiming to replicate. And don’t forget to add those classic belt-buckle scratches on the back of the guitar—show me an old guitar that doesn’t have a few of those! Once again, it’s better to be too subtle with the wear at first; you can always add more later…
CRACKLING
Once you’re happy with the nicks and scratches, it’s time for the hardest part. To cause the paint to crack. This takes time to master so it looks really natural. The thing about cutting cracks in the paint with a razor blade I’ve never really bought into – although there are probably some old Les Pauls where the paint has cracked like that. I think it will be so much prettier if you expose the color to big temperature changes. For this, a hair dryer or heat gun is used to gently heat one piece of the painted body at a time. I want to emphasize cautiously. Too much heat can cause the paint to melt, and that’s not what we’re after. Therefore, it is safest to use a hair dryer, even if it takes a while to get the paint warm enough. Then you cool it with a really good cooling spray. Spray on so that plenty of condensation forms on the paint. The colder it gets, the better. An alternative is to put the entire guitar body in the freezer overnight. It can also produce really nice crackling. If the temperature difference becomes too small, it is easy to get very small cracks – much like old porcelain. You want the cracks to be substantial, and to be properly visible. You have to try your hand at it. Feel free to do these tests on a loose piece of board, which you varnished and handled in the same way, before you start working on the fine guitar body.

And if you want to make the crackle pattern stand out more, you can try dipping a cloth into Colron Refined Wood Dye (a type of wood stain). The shade “Jacobean Dark Oak” is said to work well. I couldn’t find that specific one, but I managed to get a medium-dark shade that corresponded to a different type of wood. You apply a generous amount of the liquid to a cloth, spread it over the guitar body, and then wipe away the excess after a short while.
It worked exceptionally well—especially for darkening the bare wood areas that were exposed after I scraped off the lacquer in a few spots. Furthermore, the lacquer took on a nice, subtle yellow tint from this treatment.
Regarding “relicing,” in previous issues of MM we have covered how to age or relic both metal hardware and plastic components. The latter article can actually be found on the Musikermagasinet website. As for metal hardware, that article is unfortunately not available online; however, in short, the process can be described in two steps. In step one, you use electrolysis, and in step two, you employ a liquid typically used for etching circuit boards: sodium persulfate. For the electrolysis, you dissolve a couple of tablespoons of table salt in hot water and pour the mixture into a plastic container—an empty ice cream tub works perfectly.



Naturally, we treat the screws for the bridge, pickguard, and other components so that only the heads rust. The threads remain protected by the wood and should not be rusty—a common issue, unfortunately, with screws found on factory-aged (“relic”) instruments. The easiest method is to screw them all into a piece of cardboard (a pizza box works perfectly) so that only the heads are exposed, then treat the heads with sodium persulfate, following all the proper procedures.
ASSEMBLING
So, finally, it’s time to assemble the whole thing. This time, we got some help from the eminent Åke Björnstad—a.k.a. “Gitarrmakaren” (The Guitar Maker)—with drilling the holes in the neck. While it’s perfectly possible to do this freehand, using a drill press makes the process much easier, ensuring the holes are perfectly straight and parallel.

Then, of course, there are all the holes to drill for the pickguard, the bridge, and the control plate. We don’t need to go into all of this in detail, but the “ferrules”—the metal bushings installed on the back of the body to prevent the string ends from eating into the wood—generally come in two types: with or without a rim (or “lip”). The ones I used for this build have a rim, which means they protrude slightly from the back of the guitar. If you like, you can countersink the six holes on the back just a tiny bit—as I’ve done on a couple of previous builds—and then press the bushings in so that the rim sits flush with the wood. That usually works. Otherwise, you can simply tap them in. This might leave a few marks in the finish, but in this case, that’s exactly the kind of thing we’re looking for.

When it came to sorting out the nut, we once again enlisted the help of Åke Björnstad; he did a fantastic job, filing a piece of moose bone into the finest nut in town.
SUMMARY
Then, of course, there’s the matter of avoiding the repetition of mistakes others have already made. Looking back, I probably could have invested even more time in the preparatory work, and perhaps I should have applied a generous amount of pore filler. Also, a gloss primer might have been a better choice—if, that is, one is going to use a primer at all.
Overall though, I think the end result was really cool. I really like the light blue color, and it was given a nice yellowed character by the Coron stain. In addition, the parts where I scraped the wood bare were really nicely aged by the same liquid. I’m also really happy with the cracking, although the cracks could have been a notch more obvious. But it turned out to be a really nice guitar, if you like worn guitars. Plus, it actually sounds great. And that is the very best.